Hydrostatic test of polypropylene lined components based on 400 mm stud spacing

WANG Zhenqing, ZHANG Xiangxiang, ZHANG Hao, TAO Yuanqing

School of Civil EngineeringHenan University of TechnologyZhengzhou 450001HenanChina

Abstract:In order to solve the problem of water-proof and moisture‐proof underground granarya 10 mm thick polypropylene plastic plate was selectedwhich was lined with 400 mm plastic studs in the granary to form a waterproof memberand the member was subjected to a hydraulic test to study its mechamical performance under water pressure.The results showed thatAt a stud spacing of 400 mmthe weld failure occured when the hydraulic bearing capacity of the plastic lining reached 38 kPapressure droped to 18 kPaWhen the load continued to 26 kPathe stud wire slipping failure occuredpressure droped to 17 kPaThe final load reached 26 kPa when the plastic plate was broken. Under the action of water pressurethe mid-span displacement of the four nodes of the waterproof plastic plate increased with the increase of water pressure. The maximum displacement was 12.82 mmand the displacement at the nodes changed littleand the maximum value was 0.74 mmthe stress at the nodes in the plastic plate was largerthe stress of the four-node mid-span position was small.The research results provided a reference for the waterproof design of the underground granary.

Key words:underground granary;polypropylene;hydraulic test;mechamical performance