>> English >> Current Issue >> Mechanics · Civil Engineering · Materials Science & Engineering >> 正文
Road performance of heat-shielding and wear-resistant ceramic-steel slag asphalt mixtures
Time: 2026-11-23 Counts:

Tan B, Zhang W Z, Chen P,et al.Road performance of heat-shielding and wear-resistant ceramic-steel slag asphalt mixtures[J].Journal of Henan Polytechnic University(Natural Science) ,2027,46(1):173-179.

doi:10.16186/j.cnki.1673-9787.2024080016

Received:2024/08/11

Revised:2024/10/23

Published:2026/11/23

Road performance of heat-shielding and wear-resistant ceramic-steel slag asphalt mixtures

Tan Bo1,2, Zhang Wanzhen1,2, Chen Ping1,2, Huang Chaowang3, Chen Zuhong3

1.Guangxi Key Laboratory of Green Building Materials and Construction Industrialization, Guilin University of Technology, Guilin  541004, Guangxi, China;2.School of Civil Engineering, Guilin University of Technology, Guilin  541004, Guangxi, China;3.Cangwu Highway Maintenance Center, Guangxi Zhuang Autonomous Region, Wuzhou  543100, Guangxi, China

Abstract: Objectives A heat-shielding and wear-resistant ceramic-steel slag asphalt mixture was developed to mitigate pavement distress on secondary highways subjected to heavy traffic and high temperatures, and its pavement performance was investigated. Methods  Ceramic and steel slag with particle sizes of 4.75-9.5 mm were used to replace 40% by volume of the limestone aggregate in the corresponding size fraction. The ceramic-to-steel-slag volume ratios were set at 2∶2, 1∶3, and 3∶1. The moisture stability and rutting resistance of the mixtures were evaluated using freeze-thaw splitting and rutting tests, respectively, while their heat-shielding performance and wear resistance were evaluated through indoor light-radiation and accelerated wear tests, respectively. Results  The incorporation of ceramic and steel slag increased the asphalt content of the mixtures and improved their moisture stability and rutting resistance to varying degrees. The ceramic-steel slag asphalt mixtures exhibited a significant cooling effect; however, prolonged exposure to high temperatures also increased the surface temperature. At a ceramic-to-steel-slag ratio of 2∶2, the maximum temperature difference for the 4-cm-thick surface layer was 5.9°C, indicating the best heat-shielding performance. Steel slag exhibited high strength and a rough, porous surface, resulting in strong adhesion to asphalt. The steel slag content had a pronounced effect on wear resistance, which improved progressively with increasing steel slag content. When the steel slag content was 30%, the mixture exhibited the lowest mass loss, 227.1 g, in the accelerated wear test, representing a 25.10% improvement in wear resistance compared with the conventional limestone-only asphalt mixture. Conclusions The performance of the asphalt mixtures varied with the ceramic-to-steel-slag ratio. A ratio of approximately 2∶2 is recommended because it provides a favorable balance of overall performance while facilitating construction and material proportioning.

Key words:ceramic;steel slag;asphalt mixture;heat-shielding performance;wear resistance

Lastest